Author : mitsue-stanley | Published Date : 2015-12-10

For a given temperature the strain to reach the first serration increased with decreasing strain rate most likely to occur followed by completing the test in a normal

Presentation Embed Code

Download Presentation

Download Presentation The PPT/PDF document "SERRATED YIELDING IN A NICKEL-BASE SUPER..." is the property of its rightful owner. Permission is granted to download and print the materials on this website for personal, non-commercial use only, and to display it on your personal computer provided you do not modify the materials and that you retain all copyright notices contained in the materials. By downloading content from our website, you accept the terms of this agreement.

SERRATED YIELDING IN A NICKEL-BASE SUPERALLOY Eric S. Huron Engineered: Transcript


Download Document

Here is the link to download the presentation.
"SERRATED YIELDING IN A NICKEL-BASE SUPERALLOY Eric S. Huron Engineered"The content belongs to its owner. You may download and print it for personal use, without modification, and keep all copyright notices. By downloading, you agree to these terms.

Related Documents